SURFACE-ANALYSIS OF IRON FILMS OXIDIZED AT DIFFERENT TEMPERATURES

  • Year : 1989 Author : KUMARI, SV; VAIDYAN, VK; SATHYANARAYANA, KG; MUKHERJI, PS; KOSHY, P
  • Research Area :Materials Science & Technology Division (MSTD) Journal : JOURNAL OF MATERIALS SCIENCE LETTERS
  • DOI :10.1007/BF01730137